DecayData
SearchSign in
Material10 papers · 29 citations

Plain concrete

Papers by year 1996–2024
199620102024
Co-occurring climates
  • Subarctic continental6
  • Polar maritime5
  • Alpine high-altitude3
  • Subarctic Atlantic3
  • Cold desert plateau2
  • Polar plateau2
  • Glacial proglacial2
  • Coastal industrial port1
Co-occurring phenomena
  • Freeze-thaw cycling8
  • Salt crystallisation5
  • Cover spalling (freeze-thaw)3
  • Chloride ingress1
  • Atmospheric carbonation1
  • Atmospheric rusting1
  • Carbonation1
  • Chloride-induced corrosion of rebar1
10 / 10
YearPaperClassificationCited by ↓Conf.Links
2017
Durability of steam-cured concrete with slag under the combined deterioration of freeze-thaw cycles and de-icing chemicals
Seo, Taeseok; Jung, Younsu +2 · Structural Concrete
CementitiousPlain concreteCold desert plateauSubarctic continentalChloride ingressFreeze-thaw cyclingSalt crystallisation2072%
2021
Numerical Simulation of the Effect of Freeze–Thaw Cycles on the Durability of Concrete in a Salt Frost Environment
Li, Hao; Zhang, Yuan +1 · Coatings · abstract
Plain concreteReinforced concreteCold desert plateauPolar maritimeCover spalling (freeze-thaw)Freeze-thaw cyclingSalt crystallisation888%
2024
Carbonation-Induced Corrosion Assessment for Reinforced Concrete Structures
Lau, Kingsley; Permeh, Samanbar +3 · CONFERENCE 2024 · abstract
Carbon steelPlain concreteReinforced concreteAtmospheric carbonationAtmospheric rustingCarbonationChloride-induced corrosion of rebar192%
2022
Metagenomic analysis of concrete bridge reveals a microbial community dominated by halophilic Bacteria and Archaea
Kiledal, E. Anders; Shaw, Mark +2 · abstract
Plain concreteReinforced concreteCoastal industrial portHalophilic biofilm (cyanobacteria)Microbial growthSalt crystallisation078%
2009
THE COMPARISON OF THE FREEZE-THAW RESISTANCE OF CONCRETE EXPOSED TO ICE COVERED SEA FOR 20 YEARS AND CONCRETE WITH FREEZE-THAW TEST
KATO, Rina; AYUTA, Koichi +1 · Cement Science and Concrete Technology
Plain concreteReinforced concretePolar maritimeFreeze-thaw cycling085%
1996
Round-robin tests on concrete frost resistance
Unattributed · Freeze-Thaw Durability of Concrete
Plain concreteReinforced concreteAlpine high-altitudePolar maritimePolar plateauSubarctic AtlanticSubarctic continentalCover spalling (freeze-thaw)Freeze-thaw cycling072%
1996
Influence of water quality on the frost resistance of concrete
Unattributed · Freeze-Thaw Durability of Concrete
Plain concreteReinforced concreteAlpine high-altitudeGlacial proglacialPolar maritimeSubarctic continentalFreeze-thaw cycling075%
1996
On the service life of concrete exposed to frost action
Unattributed · Freeze-Thaw Durability of Concrete
Plain concreteReinforced concreteAlpine high-altitudeGlacial proglacialPolar plateauSubarctic continentalFreeze-thaw cycling072%
1996
Three different methods for testing the freeze-thaw resistance of concrete with and without de-icing salt: European round-robin test
Unattributed · Freeze-Thaw Durability of Concrete
Plain concreteReinforced concretePolar maritimeSubarctic AtlanticSubarctic continentalCover spalling (freeze-thaw)Freeze-thaw cyclingSalt crystallisation085%
—
Investigation of freeze-thaw durability of pervious concrete
Tahiri, Iliass · abstract
Plain concreteSubarctic AtlanticSubarctic continentalTemperate continental urbanFreeze-thaw cyclingSalt crystallisation092%